Alloy Pipe
Hastelloy B3 pipe performs better in terms of strength and corrosion resistance at high temperatures compared with traditional Hastelloy. B3 alloy has excellent stability and durability, especially in oxidizing and reducing environments, as well as corrosive environments such as strong acid and strong alkali.
Big fire special steel, high strength steel plate, steel industry supply and demand, steel suppliers
Hastelloy B3 is a nickel-based high-temperature alloy mainly consisting of nickel, molybdenum, cobalt and other elements, of which the nickel content is about 65%. This alloy material is optimized on the basis of Hastelloy B2. By improving the thermal stability of the material, it significantly enhances the corrosion resistance, while also effectively improving the hot forming and cold forming performance. In recent years, Hastelloy B3 pipe has been increasingly used in the production and manufacturing of chemical equipment. Hastelloy B3 material has many unique properties. Its high elongation provides favorable conditions for cold forming operations. Compared to austenitic stainless steel, Hastelloy B3 material is harder and therefore needs greater pressure during cold forming or step forming processes.
Product Parameters
Product Name | Hastelloy B-3 Pipe | |
Outer Diameter | Round Pipe | 4mm-200mm |
Square Pipe | 10*10mm-100*100mm | |
Rectangular Pipe | 10*20mm-50*100mm | |
Wall Thickness | 0.6mm-6.0mm | |
Length | 1-6 meters, Length can be customized | |
Standard | ASTM, AISI, JIS, GB, DIN, EN, etc. | |
Surface | Black, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc. | |
Certificate | ISO, SGS, BV | |
Production Technology | Hot Rolling, Cold Rolling |
Chemical Composition
C | Al | Si | P | S | Ti | V | Cr | Mn | Fe | Co | Ni | Cu | Zr | Nb | Mo | Ta | W | Not MO |
0.01 max | 0.5 max | 0.10 max | 0.03 max | 0.01 max | 0.2 max | 0.2 max | 1.0 - 3.0 | 3.0 max | 1.0 - 3.0 | 3.0 max | 65.0 min | 0.2 max | 0.1 max | 0.2 max | 27.0 - 32.0 | 0.2 max | 3.0 max | 94.0 - 98.0 |
Mechanical Properties
Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation% in 2 inches |
110 | 51 | 40 |
Physical Performance
Units | Temperature in°C | |
Density | 9.22 g/cm³ | Room |
Specific Heat | 0.089 Kcal/kg.C | Room |
Melting Range | 1370-1418°C | - |
Modulus of Elasticity | 216 KN/mm² | Room |
Electrical Resistivity | 137 µΩ.cm | Room |
Coefficient of Expansion | 10.6 µm/m °C | 25 - 100° |
Thermal Conductivity | 11.2 w/m-° K | Room |
Scope of Application
B- 3 is used in chemical processes, vacuum furnaces, mechanical parts in reduced pressure environments, etc.
In general, our online service time is Beijing time: 8:00-22:00, after 22:00, we will reply to your inquiry during the next working day.
The inner layer has a waterproof paper outer layer with iron packaging and is fixed with a fumigation wooden pallet. It can effectively protect products from corrosion during ocean transportation.
Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.
You need to provide the grade, width, thickness, coating and the number of tons you need to purchase.
Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.
Prices vary from period to period due to cyclical changes in the price of raw materials.
We have ISO 9001, SGS, EWC and other certifications.
In general, our delivery time is within 30-45 days, and may be delayed if the demand is extremely large or special circumstances occur.